Round Ring Block Arc Permanent Ferrite Magnet

Inkcazelo emfutshane:

Imilinganiselo: Iyakwazi ukwenzeka

IBakala: Y10, Y28, Y30, Y30BH, Y35

Ubume: Round / Cylinder / Block / Ring / Arc

Ubuninzi: 4.7-5.1g/cm³


Iinkcukacha zeMveliso

Iithegi zeMveliso

Ingcaciso yeMveliso

i-ferrite-magnet-5

Imagnethi yeFerrite (ekwabizwa ngokuba yimagnethi yeceramic) yimagnethi esisigxina.
Ikakhulu ziyi-Strontium esekelwe (i-SrFe2O3), eyenziwe kunye ne-Strontium Carbonate additive ukunyusa ukusebenza kwi-Barium ephelelwe lixesha (BaFe2O3).
Amandla abo alungileyo okunyanzela avela kwikristale ephezulu ye-anisotropy ye-strontium iron oxide. Nangona kunjalo, iindawo ze-isotropic nazo zinokuveliswa apho kufuneka i-multi-pole magnetization elula kwaye elula.
Ngokubhekiselele kwiimpawu zombane, ukuxhathisa kwe-ferrite kukhulu kakhulu kuneyentsimbi kunye ne-alloy materials magnetic, kwaye ineempawu eziphezulu ze-dielectric.
Iipropathi zemagneti zeferrite zikwabonisa ukufikeleleka okuphezulu kumaza aphezulu.
I-Ferrite ayiqhubeki kwaye inokumelana okuphezulu ngokuchasene nokubola, i-asidi, iityuwa, kunye nezinto zokuthambisa. Iimilo eziqhelekileyo zilula, ezifana nediski, iibhloko, iisilinda, imisesane, kunye neearcs.
Iimagnethi zeFerrite ziqhele ukusetyenziswa kwizicelo ezahlukeneyo kumashumi eminyaka adlulileyo, njengezandisi-lizwi, iimotor, kunye neejenereyitha.

Iimpawu zemagnethi zeSintered Ferrite (iMigangatho yaseTshayina)

IBanga

Remanence Induction
(Br)

Ukunyanzeliswa kwamandla
(Hcb)

Amandla oNyanzelo lwangaphakathi
(Hcj)

Max.Energy Product
(BH)ubuninzi

mT

Gs

k/am

kOe

k/am

kOe

kJ/m³

MGOe

Y10

200-235

2000-2350

125-160

1570-2010

210-280

2640-3520

6.5-9.5

0.8-1.2

Y25

360-400

3600-4000

135-170

1700-2140

140-200

1760-2510

22.5-28.0

2.8-3.5

Y30

370-400

3700-4000

175-210

2200-2640

180-220

2260-2770

26.0-30.0

3.3-3.8

Y30BH

380-400

3800-4000

230-275

2890-3460

235-290

2950-3650

27.0-32.5

3.4-4.1

Y33

410-430

4100-4300

220-250

2770-3140

225-255

2830-3210

31.5-35.0

4.0-4.4

Y35

400-420

4000-4200

160-190

2010-2380

165-195

2070-2450

30.0-33.5

3.8-4.2

IiPropati zeNdawo zeSintered Ferrite

I-Coefficient yeTemp ye-Br

0-0.18 ~ -0.2 %/℃

I-Coefficient yeTemp ye-Hcj

0.25-0.4%/℃

Ukuxinana

4.7-5.1 g/cm³

Ukuxhathisa koMbane

>10⁴ μΩ • cm

Vickers Ukuqina

400-700 Hv

I-Thermal Conductivity

0.029 W/m • ℃

Curie Temp

450-460℃

I-Coefficient yoKwandiswa kweThermal

9-10x10-6/℃ (20-100℃) ⟂C

Ubushushu obucacileyo

0.62-0.85 J/g • ℃

Max. ITemp yokuSebenza

1 -40 ~ 250 ℃

Ukugoba Ukumelana

5-10 Kgf/mm2

I-Compressive Resitance

68-73 mm2


  • Ngaphambili:
  • Okulandelayo:

  • Bhala umyalezo wakho apha kwaye uwuthumele kuthi